Mahsulotni tanishtirish

To'g'ri tikuvli arc payvandlangan trubka va spiral yostiqsimon trubani tayyorlash uchun nima farq qiladi?

LSAW va SSAW - arraning o'zgarishi (yoyilgan arc payvandlangan) quvur. Ularning orasidagi farq payvandlash usuli. Uzunlamasın tikuvda arc payvandlangan trubkada payvandlash uzunlamasina, demak po'latdan yasalgan po'latdan va payvand chokni uzunlashtiradi.

 

SSAW turida po'lat palillar spiral chavandoz bo'lib, palana (chiziq) naychaning shaklida ushlab turilishi uchun spiral payvanddir. Quvurlar asosan neft va gaz tashish uchun ishlatiladi. Boshqa tomondan, birinchi navbatda, chambarchas, birinchi navbatda neft va gaz qidiruv ishlari bo'yicha qo'llaniladi.

Spiral po'lat quvurlar(SSAW quvurlari) va tekis tikuv po'lat quvurlari suv ta'minotida, qurilish va boshqa sohalarda keng qo'llaniladi, ammo ular orasida ikki farq bor.

1. Turli xil bosimli imkoniyatlar

Spelal po'lat quvurlarning kuchi odatda tekis tikuvli po'lat quvurlardan yuqori. Asosiy ishlab chiqarish jarayoni Arc payvandlash suvini to'ldiradi. Spiral payvandlangan po'lat quvurlar bir xil kenglik buyumlaridan turli diametrli po'lat quvurlar ishlab chiqarishi yoki kattaroq diametr ishlab chiqaradigan po'lat quvurlar ishlab chiqarish uchun tor tendentsiyalardan foydalanadi.

2. Turli xil xususiyatlar

Spelal po'lat quvurlar xususiyatlari odatda 219 mm dan yuqori va ularning aksariyati katta diametrli. To'g'ri tikuv po'latli quvurlarning xususiyatlari asosan kichik diameter, ammo ba'zi ishlab chiqaruvchilar ham katta diametrlarga ega.

 

Ssaw uglerod trubkasini standart va sinflashtirish

Klassifikatsiya

Standart

Asosiy mahsulotlar

Chiziq quvuri

API 5L psip1 / 2

Chiziq quvuri

Qopqoq

API 5CT / ISO 11960 PSL1

Neft va tabiiy gaz sanoatining quduqlari uchun qoplama yoki naycha sifatida foydalanish uchun po'lat quvur

Suyuqlik xizmati uchun po'lat quvur

ASTM A53

Qora va issiq xalalli galvanizli payvandlangan payvandlangan va choksiz po'lat quvur

BS en 10217-2

Bosim maqsadlari uchun perel oqimlar - etkazib berish texnik shartlari - Qismlikdagi haroratli xususiyatlari va haroratli haroratli po'lat quvurli naychalar

BS en 10217-5

Bosim maqsadlari uchun payvandlangan po'latdan yasalgan texnik shartlar - Beshinchi: Tozalangan arc haroratli harorat xususiyatlari bilan qotishma bo'lmagan va qotishmali naychalarni payvandlangan

Oddiy tuzilish uchun po'lat quvur

ASTM A252

Payvandlangan va choksiz po'latdan yasalgan krep

BS en 10219-1

Sovuq shakllangan sun'iy bo'lmaganlar va nozik donli po'choqlarning tarkibiy ichi bo'sh joylari - Qism: texnik etkazib berish shartlari

BS en 10219-2

Sovuq shakllangan sun'iy bo'lmaganlar va nozik donli po'latlarning tarkibiy ichi bo'sh joylari - Qisqichbaqasi2: Bardoshlik dimvaslar va bo'lim xususiyatlari

SSSAW po'lat quvurining kimyoviy tahlili va mexanik xususiyatlari

Standart Baho Kimyoviy tarkibi (maksimal)% Mexanik xususiyatlar (min)
C SiName mn P S Zinarli kuch (MPA) Kuch berish kuchi (MPA)
API 5ct h40 - - - - 0.030 417 417
J55 - - - - 0.030 517 517
K55 - - - - 0.300 655 655
API 5L psip1 A 0.22 - 0.90 0.030 0.030 335 335
B 0.26 - 1.20 0.030 0.030 415 415
X42 0.26 - 1.30 0.030 0.030 415 415
X46 0.26 - 1.40 0.030 0.030 435 435
X52 0.26 - 1.40 0.030 0.030 460 460
X56 0.26 - 1.40 0.030 0.030 490 490
X60 0.26 - 1.40 0.030 0.030 520 520
X65 0.26 - 1.45 0.030 0.030 535 535
X70 0.26 - 1.65 0.030 0.030 570 570
API 5L PSL2 B 0.22 0.45 1.20 0.025 0.015 415 415
X42 0.22 0.45 1.30 0.025 0.015 415 415
X46 0.22 0.45 1.40 0.025 0.015 435 435
X52 0.22 0.45 1.40 0.025 0.015 460 460
X56 0.22 0.45 1.40 0.025 0.015 490 490
X60 0.12 0.45 1.60 0.025 0.015 520 520
X65 0.12 0.45 1.60 0.025 0.015 535 535
X70 0.12 0.45 1.70 0.025 0.015 570 570
X80 0.12 0.45 1.85 0.025 0.015 625 625
ASTM A53 A 0.25 0.10 0.95 0.050 0.045 330 330
B 0.30 0.10 1.20 0.050 0.045 415 415
ASTM A252 1 - - - 0.050 - 345 345
2 - - - 0.050 - 414 414
3 - - - 0.050 - 455 455
En 10217-1 P195tr1 0.13 0.35 0.70 0.025 0.020 320 320
P195tr2 0.13 0.35 0.70 0.025 0.020 320 320
P235tr1 0.16 0.35 1.20 0.025 0.020 360 360
P235tr2 0.16 0.35 1.20 0.025 0.020 360 360
P265tr1 0.20 0.40 1.40 0.025 0.020 410 410
P265tr2 0.20 0.40 1.40 0.025 0.020 410 410
En 10217-2 P195g 0.13 0.35 0.70 0.025 0.020 320 320
P235g 0.16 0.35 1.20 0.025 0.020 360 360
P265g 0.20 0.40 1.40 0.025 0.020 410 410
En 10217-5 P235g 0.16 0.35 1.20 0.025 0.020 360 360
P265g 0.20 0.40 1.40 0.025 0.020 410 410
En 10219-1 S235JRH 0.17 - 1.40 0.040 0.040 360 360
S275JOH 0.20 - 1.50 0.035 0.035 410 410
S275J2H 0.20 - 1.50 0.030 0.030 410 410
S355JOH 0.22 0.55 1.60 0.035 0.035 470 470
S355J2H 0.22 0.55 1.60 0.030 0.030 470 470
S355K2H 0.22 0.55 1.60 0.030 0.030 470 470

Spiral yostiqchani suvga botirdi

SSAW Steel Pipe

Spiral tikilgan po'lat quvur

Spiral tikuvning ishlab chiqarish jarayoni yoyni pishirilgan temir quvurlar, temir va tashqi payvandlash, kesish, tugatish, zangni tozalash va purkagichni o'z ichiga oladi. Payvandni qayta ishlashni tugatgandan so'ng, zaryadirmaydigan sinov, shuningdek, paypoq tanasining yaxlitligi sifatini ta'minlash uchun talab qilinadi. Odatda ishlatilgan zararsiz sinov usullari rentgenografik sinov, ultratovush testi, magnit zarracha sinovlari va boshqalarga kiradi.

SSAW carbon Pipe

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

Gnee mahsulot sertifikati

Gnee product certificate

Gne kompaniyasining jamoasi

Gnee Company Team

Gne Group NeSC ko'rgazmasida ishtirok etdi

Gnee Group participated in the NECC exhibition​

Gne Mijozga tashrif

Gnee Customer visit

Gne zavod muhitiproduct-1-1

​ Gnee Factory environment  ​​

Gnee qadoqlash va etkazib berishproduct-1-1

​ Gnee Packaging and shipping  ​

Issiq teglar: SSAW po'lat quvuri, Xitoy SSSAW po'lat quvur ishlab chiqaruvchilar, etkazib beruvchilar, fabrikalar

So'rov yuborish

whatsapp

Telefon

Elektron pochta

So'rov