Kimyoviy xossalari
X daraja60-PSL1 Neft va gaz quvurlari Kimyoviy tarkibi (%)
| Tarkibi | C * | Mn* | P | S | Cr | Ni | Cu | Mo | B | Ko'proq | |
|---|---|---|---|---|---|---|---|---|---|---|---|
| Choksiz quvur | Min | - | - | - | - | - | - | - | - | - | Nb+V+Ti 0 dan kichik yoki unga teng.15* |
| Maks | 0.28 | 1.4 | 0.03 | 0.03 | 0.5 | 0.5 | 0.5 | 0.15 | 0.001 |
| Tarkibi | C * | Mn* | P | S | Cr | Ni | Cu | Mo | B | Ko'proq | |
|---|---|---|---|---|---|---|---|---|---|---|---|
| Payvandlangan quvur | Min | - | - | - | - | - | - | - | - | - | Nb+V+Ti 0 dan kichik yoki unga teng.15* |
| Maks | 0.26 | 1.4 | 0.03 | 0.03 | 0.5 | 0.5 | 0.5 | 0.15 | 0.001 |
X60N-PSL2 darajasi uglerodli po'lat quvurining kimyoviy tarkibi (%)
| Tarkibi | C * | Si* | Mn* | P | S | Cr* | Ni* | Cu* | Mo* | Ti* | V * | Nb* | B | Ko'proq | |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Choksiz quvur, payvandlangan quvur | Min | - | - | - | - | - | - | - | - | - | - | - | - | - | Nb+V+Ti 0 dan kichik yoki unga teng.15* |
| Maks | 0.24 | 0.45 | 1.4 | 0.025 | 0.015 | 0.5 | 0.5 | 0.5 | 0.5 | 0.04 | 0.1 | 0.05 | 0.001 |
X60Q-PSL2 markali choksiz po'lat quvurlari kimyoviy tarkibi (%)
| Tarkibi | C * | Si* | Mn* | P | S | Cr* | Ni* | Cu* | Mo* | B | Ko'proq | |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Choksiz quvur, payvandlangan quvur | Min | - | - | - | - | - | - | - | - | - | - | Nb+V+Ti 0 dan kichik yoki unga teng.15* |
| Maks | 0.18 | 0.45 | 1.7 | 0.025 | 0.015 | 0.5 | 0.5 | 0.5 | 0.5 | 0.001 |
Yonuvchan suyuqliklar uchun X60M-PSL2 darajali quvurlar kimyoviy tarkibi (%)
| Tarkibi | C * | Si* | Mn* | P | S | Cr* | Ni* | Cu* | Mo* | B | Ko'proq | |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Payvandlangan quvur | Min | - | - | - | - | - | - | - | - | - | - | Nb+V+Ti 0 dan kichik yoki unga teng.15* |
| Maks | 0.12 | 0.45 | 1.6 | 0.025 | 0.015 | 0.5 | 0.5 | 0.5 | 0.5 | 0.001 |
X daraja65-PSL1 choksiz quvurlar kimyoviy tarkibi(%)
| Tarkibi | C * | Mn* | P | S | Cr | Ni | Cu | Mo | B | Ko'proq | |
|---|---|---|---|---|---|---|---|---|---|---|---|
| Choksiz quvur | Min | - | - | - | - | - | - | - | - | - | Nb+V+Ti 0 dan kichik yoki unga teng.15* |
| Maks | 0.28 | 1.4 | 0.03 | 0.03 | 0.5 | 0.5 | 0.5 | 0.15 | 0.001 |
| Tarkibi | C * | Mn* | P | S | Cr | Ni | Cu | Mo | B | Ko'proq | |
|---|---|---|---|---|---|---|---|---|---|---|---|
| Payvandlangan quvur | Min | - | - | - | - | - | - | - | - | - | Nb+V+Ti 0 dan kichik yoki unga teng.15* |
| Maks | 0.26 | 1.45 | 0.03 | 0.03 | 0.5 | 0.5 | 0.5 | 0.15 | 0.001 |
X65Q-PSL2 darajasi uglerodli po'lat quvurlari kimyoviy tarkibi (%)
| Tarkibi | C * | Si* | Mn* | P | S | Cr* | Ni* | Cu* | Mo* | B | Ko'proq | |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Choksiz quvur, payvandlangan quvur | Min | - | - | - | - | - | - | - | - | - | - | Nb+V+Ti 0 dan kichik yoki unga teng.15* |
| Maks | 0.18 | 0.45 | 1.7 | 0.025 | 0.015 | 0.5 | 0.5 | 0.5 | 0.5 | 0.001 |
X65M-PSL2 darajasi Karbonli po'latdan yuqori haroratli choksiz quvurlar Kimyoviy tarkibi (%)
| Tarkibi | C * | Si* | Mn* | P | S | Cr* | Ni* | Cu* | Mo* | B | Ko'proq | |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Payvandlangan quvur | Min | - | - | - | - | - | - | - | - | - | - | Nb+V+Ti 0 dan kichik yoki unga teng.15* |
| Maks | 0.18 | 0.45 | 1.6 | 0.025 | 0.015 | 0.5 | 0.5 | 0.5 | 0.5 | 0.001 |

Mexanik xususiyatlar
Yuqori bosimli gaz tashish uchun X60-PSL1 toifali quvur Mexanik xususiyatlar
| Turi | Mustahkamlik chegarasi σb Mpa |
Hosildorlik nuqtasi σs Mpa |
Tanaffus paytida cho'zilish δ % |
|---|---|---|---|
| Choksiz quvur, payvandlangan quvur | 520 dan katta yoki unga teng | 415 dan katta yoki unga teng | * |
Neft va gaz uchun X60N-PSL2 sinf quvurlari Mexanik xususiyatlar
| Turi | Sinov harorati | Mustahkamlik chegarasi σb Mpa |
Hosildorlik nuqtasi σs Mpa |
Tanaffus paytida cho'zilish δ % |
Ta'sir yutilgan energiya KV2 J |
|---|---|---|---|---|---|
| Choksiz quvur, payvandlangan quvur | 520~760 | 415~565 | * | ||
| OD 20 dan kam yoki unga teng | 0 daraja | 27 dan katta yoki teng | |||
| OD>20~30 | 0 daraja | 27 dan katta yoki teng | |||
| OD>30~36 | 0 daraja | 40 dan katta yoki teng | |||
| OD>36~48 | 0 daraja | 40 dan katta yoki teng | |||
| OD>48~56 | 0 daraja | 40 dan katta yoki teng | |||
| OD>56~84 | 0 daraja | 40 dan katta yoki teng |
X60Q-PSL2 darajasi uglerodli po'lat quvur liniyasi mexanik xususiyatlari
| Turi | Sinov harorati | Mustahkamlik chegarasi σb Mpa |
Hosildorlik nuqtasi σs Mpa |
Tanaffus paytida cho'zilish δ % |
Ta'sir yutilgan energiya KV2 J |
|---|---|---|---|---|---|
| Choksiz quvur, payvandlangan quvur | 520~760 | 415~565 | * | ||
| OD 20 dan kam yoki unga teng | 0 daraja | 27 dan katta yoki teng | |||
| OD>20~30 | 0 daraja | 27 dan katta yoki teng | |||
| OD>30~36 | 0 daraja | 40 dan katta yoki teng | |||
| OD>36~48 | 0 daraja | 40 dan katta yoki teng | |||
| OD>48~56 | 0 daraja | 40 dan katta yoki teng | |||
| OD>56~84 | 0 daraja | 40 dan katta yoki teng |
X60M-PSL2 darajasi Neft va gaz uzatish trubkasi Mexanik xususiyatlar
| Turi | Sinov harorati | Mustahkamlik chegarasi σb Mpa |
Hosildorlik nuqtasi σs Mpa |
Tanaffus paytida cho'zilish δ % |
Ta'sir yutilgan energiya KV2 J |
|---|---|---|---|---|---|
| Payvandlangan quvur | 520~760 | 415~565 | * | ||
| OD 20 dan kam yoki unga teng | 0 daraja | 27 dan katta yoki teng | |||
| OD>20~30 | 0 daraja | 27 dan katta yoki teng | |||
| OD>30~36 | 0 daraja | 40 dan katta yoki teng | |||
| OD>36~48 | 0 daraja | 40 dan katta yoki teng | |||
| OD>48~56 | 0 daraja | 40 dan katta yoki teng | |||
| OD>56~84 | 0 daraja | 40 dan katta yoki teng |

Tabiiy gaz uchun X65-PSL1 toifali choksiz quvur Mexanik xususiyatlar
| Turi | Mustahkamlik chegarasi σb Mpa |
Hosildorlik nuqtasi σs Mpa |
Tanaffus paytida cho'zilish δ % |
|---|---|---|---|
| Choksiz quvur, payvandlangan quvur | 535 dan katta yoki unga teng | 450 dan katta yoki teng | * |
X65Q-PSL2 darajasi uglerodli po'lat quvur liniyasi mexanik xususiyatlari
| Turi | Sinov harorati | Mustahkamlik chegarasi σb Mpa |
Hosildorlik nuqtasi σs Mpa |
Tanaffus paytida cho'zilish δ % |
Ta'sir yutilgan energiya KV2 J |
|---|---|---|---|---|---|
| Choksiz quvur, payvandlangan quvur | 535~760 | 450~600 | * | ||
| OD 30 dan kam yoki unga teng | 0 daraja | 27 dan katta yoki teng | |||
| OD>30~48 | 0 daraja | 40 dan katta yoki teng | |||
| OD>48~84 | 0 daraja | 54 dan katta yoki teng |
X65M-PSL2 darajasi choksiz po'lat quvur liniyasi mexanik xususiyatlari
| Turi | Sinov harorati | Mustahkamlik chegarasi σb Mpa |
Hosildorlik nuqtasi σs Mpa |
Tanaffus paytida cho'zilish δ % |
Ta'sir yutilgan energiya KV2 J |
|---|---|---|---|---|---|
| Payvandlangan quvur | 535~760 | 450~600 | * | ||
| OD 30 dan kam yoki unga teng | 0 daraja | 27 dan katta yoki teng | |||
| OD>30~48 | 0 daraja | 40 dan katta yoki teng | |||
| OD>48~84 | 0 daraja | 54 dan katta yoki teng |
Ilova:
X65 ning yuqori quvvati va bosimga chidamliligi tufayli u odatda yuqori bosim va harorat sharoitida neft va gazni tashish quvurlarida, ayniqsa transport tizimida uzoqroq masofalar va murakkab erlar talab qilinadigan ilovalarda qo'llaniladi.