Dec 10, 2025 Xabar QOLDIRISH

B darajali quvur uchun bosim darajasi qanday

API 5L Grade B quvurlari uchun bosim darajasi qanday?

API 5L Grade B trubkasi neft va gaz quvurlarini uzatish uchun keng tarqalgan quvurdir. Bu L245 quvuri sifatida ham tanilgan (qarang: ISO 3183). Minimal oqish quvvati 245 MPa (35,500 psi).

 

‌API 5L Gr.B choksiz po'lat quvurlaridan ishlab chiqariladiyuqori-sifatli uglerodli po'lat yoki past-qotishma po'latdan yasalgan ignalarissiq{0}}prokat yoki sovuq{1}}chizish jarayonlari orqali. Asosiy spetsifikatsiyalarga quyidagilar kiradi:

‌Kimyoviy tarkibi‌:

Uglerod (C) 0,28% dan kam yoki unga teng

Marganets (Mn) 1,20% dan kam yoki teng

‌Mexanik xususiyatlar‌:

Oqim kuchi 241 MPa dan katta yoki unga teng

Kuchlanish kuchi: 413-517 MPa

‌Payvandlash nazorati‌:

Uglerod ekvivalenti (Ceq) odatda 0,43% dan kam yoki unga teng bo'lishi payvandlanishni ta'minlaydi

 

API 5L B darajali quvurlar jadvali

NB DN OD (mm) Quvurlar jadvali
SCH 5 SCH 10 SCH
20
SCH 30 SCH 40 SCH 60 SCH 80 SCH 100 SCH 120 SCH 160
3/4" 20 26.67 1.65 2.11 x 2.41 2.87 x 3.91 x 4.32 5.56
1" 25 33.40 1.65 2.77 x 2.90 3.38 x 4.55 x 5.08 6.35
1.1/2" 40 48.26 1.65 2.77 x 3.18 3.68 x 5.08 x 5.72 7.14
2" 50 60.32 1.65 2.77 x x 3.91 x 5.54 x 6.35 8.74
2.1/2" 65 73.02 2.11 3.05 x x 5.16 x 7.01 x 7.62 9.53
3" 80 88.9 2.11 3.05 x x 5.49 x 7.62 x 8.89 11.13
4" 100 114.3 2.11 3.05 x x 6.02 x 8.56 x 11.10 13.49
5" 125 141.3 5.77 3.4 x x 6.55 x 9.53 x 12.70 15.88
6" 150 168.27 2.77 3.4 x x 7.11 x 10.97 x 14.27 18.26
8" 200 219.07 2.77 3.76 6.35 7.04 8.18 12.7 12.70 15.06 18.24 23.01
10" 250 273.05 3.4 4.19 6.35 7.8 9.27 12.7 15.06 18.24 21.41 28.58
12" 300 323.85 4.19 4.57 6.35 8.38 10.31 12.7 17.45 21.41 25.40 33.32

 

sinov va tekshirish

O'lchovli og'ishlar

sirt sifati

kimyoviy tarkibi tahlili

mexanik xususiyatlarni tekshirish

buzilmaydigan sinovlar-

inspection

 

API 5L GRB Gaz va neft quvurlari zavodi

API 5L GRB Pipeline Factory

So'rov yuborish

whatsapp

Telefon

Elektron pochta

So'rov