API X70 tarkibining tarkibi nima?
X70 satr quvuri - bu neft va gaz sohasida ishlatiladigan uzatish quvurining turi va birligiga (IE 485 MPA) bir-biridan (IE 485 MPA) spetsifikatsiyalangan.
Kimyoviy tarkibi:
|
Baho |
Tarkibi (%) |
Cev (%) |
||||||||
|
- |
C |
Si |
Mn |
P |
S |
V |
Nb |
Ti |
B |
- |
|
X70 |
0 dan kam yoki unga teng |
0 dan kam yoki teng}. 45 |
1,70 dan kam yoki teng |
0 dan kam yoki teng}. 020 |
0 dan kam yoki unga teng. 010 |
0 dan kam yoki teng}. 06 |
0 dan kam yoki teng}. 05 |
0 dan kam yoki teng}. 06 |
0 dan kam yoki teng}. 45 |
- |
Mexanik xususiyatlar:
|
Standart |
Baho |
Zinarli kuch (MPA) |
kuch berish kuchi (MPA) |
Flexal nisbati |
cho'zish (%) |
0 ilmiy darajadagi ta'sir kuchlari Akv (j) |
Issiqlikni davolash holati |
|
API 5L |
X70 |
570 dan katta yoki unga teng |
485-605 |
0 dan kam yoki teng}. 90 |
18 |
40 dan katta yoki unga teng |
Qattiqlashish + tebrat |