Mar 22, 2024 Xabar QOLDIRISH

Spiral payvandlangan quvurlarni qoplash xususiyatlari

SSAW po'lat quvur (spiral suv osti yoyi trubkasi), spiral payvandlangan quvur

O'lchamlari:

Chiqish diametri: 219mm-3620mm

Devor qalinligi: 5mm-25.4mm

Uzunligi: 3m-12m

SSAW po'lat quvurlarining standarti va tasnifi

Tasniflash

Standart

Asosiy mahsulotlar

Quvur liniyasi

API 5L PSL1% 2f2

Chiziqli quvur

Koson

API 5CT% 2f ISO 11960 PSL1

Neft va tabiiy gaz sanoati quduqlari uchun korpus yoki quvur sifatida foydalanish uchun po'lat quvur

Suyuqlik xizmati uchun po'lat quvur ASTM A53 Qora va issiq galvanizli payvandlangan va choksiz po'lat quvur
BS EN10217-2} Bosim uchun payvandlangan po'lat quvurlar - etkazib berishning texnik shartlari - 2-qism: Belgilangan yuqori haroratli qotishma va qotishma po'latdan yasalgan quvurlar
BS EN10217-5} Bosim maqsadlari uchun payvandlangan po'lat quvurlar - etkazib berishning texnik shartlari - 5-qism: ko'tarilgan harorat xususiyatlariga ega bo'lgan suv osti yoyi bilan payvandlangan qotishmagan va qotishma po'lat quvurlar
Oddiy tuzilma uchun po'lat quvur ASTM A252 Payvandlangan va choksiz po'lat quvur qoziqlari
BS EN10219-1} Qotishtirilmagan va nozik taneli po'latlarning sovuq shakllangan payvandlangan konstruktiv bo'shliqlari - 1-qism: Texnik etkazib berish shartlari
BS EN10219-2 Qotishtirilmagan va nozik taneli po'latlarning sovuq shakllangan payvandlangan strukturaviy ichi bo'sh qismlari - 2-qism: tolerantlik xiraliklari va kesma xususiyatlari

SSAW po'lat quvurining kimyoviy tahlili va mexanik xususiyatlari

Standart

Baho

Kimyoviy tarkibi(maks)%

Mexanik xususiyatlar (min)

C

Si

Mn

P

S

Kuchlanish kuchi (Mpa)

Hosildorlik (Mpa)

API 5CT

h40

-

-

-

-

0.030

417

417

J55

-

-

-

-

0.030

517

517

K55

-

-

-

-

0.300

655

655

API 5L PSL1

A

0.22

-

0.90

0.030

0.030

335

335

B

0.26

-

1.20

0.030

0.030

415

415

X42

0.26

-

1.30

0.030

0.030

415

415

X46

0.26

-

1.40

0.030

0.030

435

435

X52

0.26

-

1.40

0.030

0.030

460

460

X56

0.26

-

1.40

0.030

0.030

490

490

X60

0.26

-

1.40

0.030

0.030

520

520

X65

0.26

-

1.45

0.030

0.030

535

535

X70

0.26

-

1.65

0.030

0.030

570

570

API 5L PSL2

B

0.22

0.45

1.20

0.025

0.015

415

415

X42

0.22

0.45

1.30

0.025

0.015

415

415

X46

0.22

0.45

1.40

0.025

0.015

435

435

X52

0.22

0.45

1.40

0.025

0.015

460

460

X56

0.22

0.45

1.40

0.025

0.015

490

490

X60

0.12

0.45

1.60

0.025

0.015

520

520

X65

0.12

0.45

1.60

0.025

0.015

535

535

X70

0.12

0.45

1.70

0.025

0.015

570

570

X80

0.12

0.45

1.85

0.025

0.015

625

625

ASTM A53

A

0.25

0.10

0.95

0.050

0.045

330

330

B

0.30

0.10

1.20

0.050

0.045

415

415

ASTM A252

1

-

-

-

0.050

-

345

345

2

-

-

-

0.050

-

414

414

3

-

-

-

0.050

-

455

455

UZ10217-1

P195TR1

0.13

0.35

0.70

0.025

0.020

320

320

P195TR2

0.13

0.35

0.70

0.025

0.020

320

320

P235TR1

0.16

0.35

1.20

0.025

0.020

360

360

P235TR2

0.16

0.35

1.20

0.025

0.020

360

360

P265TR1

0.20

0.40

1.40

0.025

0.020

410

410

P265TR2

0.20

0.40

1.40

0.025

0.020

410

410

UZ10217-2

P195GH

0.13

0.35

0.70

0.025

0.020

320

320

P235GH

0.16

0.35

1.20

0.025

0.020

360

360

P265GH

0.20

0.40

1.40

0.025

0.020

410

410

UZ10217-5

P235GH

0.16

0.35

1.20

0.025

0.020

360

360

P265GH

0.20

0.40

1.40

0.025

0.020

410

410

UZ10219-1

S235JRH

0.17

-

1.40

0.040

0.040

360

360

S275JOH

0.20

-

1.50

0.035

0.035

410

410

S275J2H

0.20

-

1.50

0.030

0.030

410

410

S355JOH

0.22

0.55

1.60

0.035

0.035

470

470

S355J2H

0.22

0.55

1.60

0.030

0.030

470

470

S355K2H

0.22

0.55

1.60

0.030

0.030

470

470

Spiral Welded Pipe