Quvurning nominal bosimini hisoblash usullari asosan quyidagilarni o'z ichiga oladi:
1. Quvurning kuchlanish kuchi va devor qalinligi asosida hisoblash:
Formula: Quvur bardosh bera oladigan bosim (MPa) {0}} trubaning kuchlanish kuchi (MPa) × trubaning devor qalinligi (m) / quvurning ichki diametri (m) . Misol uchun, tashqi diametri 10mm va devor qalinligi 1mm bo'lgan zanglamaydigan po'lat quvurning kuchlanish kuchi 500MPa bo'lsa, uning bosim ko'tarish qobiliyati 500 × 0,001 / 0.008=62 ,5MPa. Xavfsizlik koeffitsienti 2 bo'lsa, haqiqiy bosim ko'tarish quvvati 62,5 / 2=31,25MPa1.
2.Loyihaviy bosim va devor qalinligi asosida hisoblash:
Formula: S{0}} s2([ ]E + PY), bu erda S1 - hisoblangan qalinlik, s - dizayn haroratida zarur bo'lgan material kuchlanishi, E - payvand choki koeffitsienti. Misol uchun, agar dizayn bosimi 1MPa bo'lsa, dizayn haroratidagi material kuchlanishi 200MPa va payvandlash birlashma koeffitsienti 0,85 bo'lsa, S1=200 × 0.85 + 1=170 + 1=171MPa2. .
3.Quvurdagi suv bosimiga qarab hisoblash:
Formula: P {0}}SR / D, bu erda S - devor qalinligi, R - 0,4 × kuchlanish kuchi va D - tashqi diametr. Misol uchun, agar devor qalinligi 2 mm, kuchlanish kuchi 400 MPa va tashqi diametri 100 mm bo'lsa, u holda P=2 × 2 × 400 / 100=8MPa1.
Quvurning nominal bosimining ta'rifi va ahamiyati:
Nominal bosim uskunaning normal ishlash talablariga javob beradigan maksimal bosimni bildiradi. Uskunaning haqiqiy ish bosimi nominal bosimdan kattaroq bo'lsa, uskunaning ishlash muddati qisqartiriladi va jiddiy holatlarda xavfsizlik baxtsiz hodisalari sodir bo'ladi.
Nominal bosim mos yozuvlar haroratida quvur liniyasi tomonidan ruxsat etilgan maksimal ish bosimini anglatadi. Nominal bosimni bilish tizimning xavfsiz ishlashini ta'minlash uchun tegishli quvurlar va armaturalarni tanlashga yordam beradi.