May 16, 2024 Xabar QOLDIRISH

ERW karbonli po'lat quvur

OD (tashqi diametri): 21.3-660 mm
WT (devor qalinligi): 1.0-20mm yoki sch5, sch10, sch40, sch80, st, xs
Standart:
erw trubkasi uchun
ASTM A53 B, A106, ASTM A178, ASTM A252
API 5L X42/46/52/56/60/70
ASTM A500, ASTM A513
EN 10204/10217 S235JR, S275JR, S355, S355JR, S355J2H
efw trubkasi uchun
uglerod po'latdan yasalgan quvur: ASTM A671, ASTM A672
qotishma po'latdan yasalgan quvur: ASTM A691
Qoplama
3PE qoplamasi
3PP qoplamasi
FBE qoplamasi
Epoksi qoplama
Maxsus rasm

ERW Carbon Steel Pipe

Tashqi diametrning bardoshliligi

Standart Chiqish diametri Quvur uchining bardoshliligi Quvur tanasining bardoshliligi
API 5L

219.1-273.1

+1.6mm, -0.4mm ±0.75%
274.0-320 +2.4mm, -0.8mm ±0.75%
323.9-457 +2.4mm, -0.8mm ±0.75%
508 +2.4mm, -0.8mm ±0.75%
559-610 +2.4mm, -0.8mm ±0.75%

Devor qalinligining bardoshliligi

Standart Baho Chiqish diametri Devor qalinligi
API 5L A 219.1-457 +15%, -12.5%
B 508-610 +17.5%, -12.5%
X42-X80 508-610 +19.5%, -8%

Kimyoviy tahlil va mexanik xossalari

Standart Sinf Baho Kimyoviy tahlil (%) Mexanik xususiyatlar (min) (Mpa)
C Mn P S Mustahkamlik chegarasi Hosildorlik kuchi
API 5L PSL1 B 0.26 1.20 0.030 0.030 414 241
X42 0.26 1.30 0.030 0.030 414 290
X46 0.26 1.40 0.030 0.030 434 317
X52 0.26 1.40 0.030 0.030 455 359
X56 0.26 1.40 0.030 0.030 490 386
X60 0.26 1.40 0.030 0.030 517 414
X65 0.26 1.45 0.030 0.030 531 448
X70 0.26 1.65 0.030 0.030 565 483
PSL2 B 0.22 1.20 0.025 0.015 414 241
X42 0.22 1.30 0.025 0.015 414 290
X46 0.22 1.40 0.025 0.015 434 317
X52 0.22 1.40 0.025 0.015 455 359
X56 0.22 1.40 0.025 0.015 490 386
X60 0.22 1.40 0.025 0.015 517 414
X65 0.22 1.45 0.025 0.015 531 448
X70 0.22 1.65 0.025 0.015 565 483
X80 0.22 1.85 0.025 0.015 621 552

So'rov yuborish

whatsapp

Telefon

Elektron pochta

So'rov