X52 neft quvuri quvuriMaxsus mo'ljallanganXitoy milliy neft korporatsiyasi (CNPC) quvurlariVa keng qo'llaniladiNeft, tabiiy gaz, suv va boshqa o'rta transport loyihalari. Umumiy xususiyatlarga quyidagilar kiradi:

Diametri diapazoni: 34-ph3500 mm

Devor qalinligi: 3.0-60 mm

Ulanish usullari: Payvandlash, ulanish ulanishi va soket ulanishi

 

Diumnsioni:

1) chirishsiz: OD: 21.3-508mm wt: 2-60mm
2) HFW / ERW: OD: 21.3-508mm wt: 3.2-15.9mm
3) LSAW: OD: 406.4-1422mm WT: 6.4-44.5MM
4) SSS: OD: 219.1.1-2540 mm WT: 5.4-25.4 mm

 

API 5L X52 payvandsiz / choksiz quvurlar kimyoviy tarkibi:

X52 PSL-1 max

C 0.26

Mn 1.40

P 0.03

S 0.03

Si /

1-sinf x52 psi-2 max

C 0.12

Mn 1.70

P 0.025

S 0.015

Si 0.45

 

API 5L x52 payvandlangan / changsiz quvurlar mexanik xususiyatlari:

Baho

Hosildorlik kuchi (min.) MPa

Zinarli kuch (min.) MPa

Cho'zish

X52 PSL-1

359

455

E=1944 A 0.2 /U 0.9

X52 PSL-2

359-531

490-758

E=1944 A 0.2 / U 0.9

 

info-500-500API 5L X52 PSL1 seamless pipe for oil 

Biz bilan bog'laningAPI 5L X52 PSL1 PSL2 choksiz payvandlangan quvurpipes@gneetube.com

So'rov yuborish

whatsapp

Telefon

Elektron pochta

So'rov